884aa四虎影成人精品,99久久国产综合精品女图图等你,97在线观看永久免费视频,久久精品国产精品亚洲38,ⅵdeodesetv性欧美

您現(xiàn)在的位置:建筑結(jié)構(gòu)>> 期 刊>> 2017年>> 第12期>>正文內(nèi)容
鋁合金網(wǎng)殼結(jié)構(gòu)盤式節(jié)點(diǎn)承載力計(jì)算方法研究*
柳曉晨1,2,王元清2,石永久2,歐陽元文3,尹建3
摘 要

(1 華東建筑設(shè)計(jì)研究院有限公司, 上海  200011; 2 清華大學(xué)土木工程安全與耐久教育部重點(diǎn)實(shí)驗(yàn)室, 北京 100084; 3 上海通正鋁業(yè)工程技術(shù)有限公司, 上海  200949)

[摘要]研究鋁合金盤式節(jié)點(diǎn)在彎矩作用下的承載力計(jì)算方法,對試驗(yàn)中5種不同尺寸、不同受力桿件的盤式節(jié)點(diǎn)破壞模式進(jìn)行了分析,分別推導(dǎo)了每種破壞模式下對應(yīng)的節(jié)點(diǎn)承載力。結(jié)合ABAQUS軟件對加載過程進(jìn)行有限元模擬,給出了節(jié)點(diǎn)板及桿件由于應(yīng)力集中造成了節(jié)點(diǎn)拉力修正的系數(shù)γ。與試驗(yàn)結(jié)果的比較表明,給出的鋁合金網(wǎng)殼結(jié)構(gòu)盤式節(jié)點(diǎn)承載力簡化計(jì)算公式具有良好的實(shí)用性,而且考慮節(jié)點(diǎn)發(fā)生塊狀撕裂的脆性破壞形式而預(yù)留了一定的安全儲備,可應(yīng)用于鋁合金網(wǎng)殼結(jié)構(gòu)盤式節(jié)點(diǎn)工程設(shè)計(jì)。

[關(guān)鍵詞]鋁合金網(wǎng)殼; 盤式節(jié)點(diǎn); 承載力; 設(shè)計(jì)方法

中圖分類號:TU395文獻(xiàn)標(biāo)識碼:A文章編號:1002-848X(2017)12-0068-06

 

Calculation method study of bearing capacity of TEMCOR joints in aluminum alloy shell structures

Liu Xiaochen1,2, Wang Yuanqing2, Shi Yongjiu2, Ouyang Yuanwen 3, Yin Jian 3

(1 East China Architectural Design & Research Institute Co.,  Ltd.,  Shanghai 200011, China;  2 Key Laboratong  of Civil Engineering  Safety and Durability of China Education Ministry, Tsinghua University, Beijing 100084, China; 3 Shanghai Tongzheng Aluminum  Industry Co., Ltd.,  Shanghai 200949, China)

Abstract:In order to study  calculation method of bearing capacity of TEMCOR joints in aluminum alloy shell structures, failure modes of 5 TEMCOR joints with different sizes and members under different bending loads were analyzed. Joint bearing capacity of each failure mode was derived. With the help of ABAQUS software, the finite element method was used to simulate the loading process and the coefficient γ of the tension of the gusset plate and the rod caused by stress concentration was given. Comparison with experimental results shows that the simplified calculation formula of bearing capacity of TEMCOR joints in aluminum alloy shell structures has good feasibility, and it sets aside a certain safety margin considering the massive tear brittle failure form in joints, which can be applied to actual engineering design of TEMCOR joints in aluminum alloy shell structures.

Keywords:aluminum alloy shell structure; TEMCOR joint; bearing capacity; design method

 

*國家自然科學(xué)基金重點(diǎn)項(xiàng)目(51038006)。

 

作者簡介:柳曉晨,碩士,助理工程師,Email: lxc2013210127@163.com。